Skimmia Cream
Mechanical and Physical Description
1-Dry unit-axial compressive strength (size: 10 cm* 10cm*10cm)1
D.U.C.S=620 kgf cm-2
2-wet unit-axial compressive strength ( size: 10cm* 10cm* 10cm*)
Samples saturated in water for 48 hours ) :
W.U.C.S=415 kgf cm -2
3-Softing coefficient ( W.U.C.S:D.U.C.S)
S.C= 0.67
4-Hardness (In Mohs Scale)
H=3.5 – 3
5-Density
D=2.71gr .cm – 3
6- water absorption coefficient ( samples saturated in water for 48 hours)
W.A.C = 0.83%
7-LOSS ON CUTTING AND ABRASION ( In Laboratory Conditions )
7-1 LOSS ON CUTTING
L.O.C=2.97%
7-2 LOSS ON ABRASION ( BY THE SILICON CARBIDE 1200, 800, 200 )
L.O.A= 0.71%
Can Iran's Skimmia Cream Marble be used exterior applications in very humid climates?
What grade is Iran's Skimmia Cream Marble?
Can Iran's Skimmia Cream Marble be used in a living room?
Can Iran's Skimmia Cream Marble be used in landscaping?
Are there color variations of Iran's Skimmia Cream Marble?
What is the coefficient of friction of Chiseled Iran's Skimmia Cream Marble tiles?
Is Iran's Skimmia Cream Marble an expensive stone?
Can Iran's Skimmia Cream Marble be used outdoors?
The request includes: 1. surface finished, size 2. quantity required